High Tensile Brass Rods

High Tensile Brass Rods are engineered for demanding industrial applications requiring exceptional strength, durability, and precision. They offer excellent wear and corrosion resistance, superior machinability, and reliable performance, making them ideal for manufacturing bushings, fasteners, shafts, valves, marine components, and heavy-duty engineering parts.

  • Description
  • Chemical Composition
  • Physical Properties
  • Sizes Available

Naval Brass C46400 is nominally composed of 60% copper, 39.2% zinc and 0.8% tin. As is typical of brass alloys with the duplex alpha + beta structure, C46400 has good strength and rigidity. By substituting tin for an equal quantity of zinc, a high corrosion resistance to seawater is achieved. The addition of tin also gives the alloy an inherent resistance to dezincification, thereby further inhibiting the impingement by seawater at higher than normal temperatures. The alloy is also noted for its resistance to wear, fatigue, galling, and stress corrosion cracking.

Typical Applications:

  • BUILDERS HARDWARE: Lock Pins
  • ELECTRICAL: Precision Shipboard Equipment
  • FASTENERS: Rivets, Bolts, Nuts
  • INDUSTRIAL: Welding Rod, Condenser Plates, Structural Uses, Valve Stems, Balls, Heat Exchanger Tube, Aircraft Turn Buckle Barrels, Bearings, Dies, Golf Ball Production, Pressure Vessels, Bearings, Bushings, Hub Cones
  • MARINE: Properller Shafts, Marine Hardware, Decorative Fittings, Shafting, Propeller Shafts, Turn buckles
  • ORDINANCE: Missle Components
  • OTHER: Baffle Platesand Flanges
  • PLUMBING: Fittings

    Equivalent Specifications
  • SPECIFICATIONSDESIGNATION
    ISOCuZn38Sn1
    EuropenCuZn39Sn1
    BSCZ 133
    JISC 4640
    RussianL060-1

Chemical Composition

 CuFePbSnZn
Min/Max59.0 - 62.00.10.20.5 - 1.0Rem
Nominals60.0000--0.700039.2000

Physical Properties

Coefficient of Thermal Expansion11.8 10−6Per °F (68-572 F)
Density0.304 lb/in3 @ 68 F
Electrical Conductivity26 %IACS @ 68 F
Electrical Resistivity39.9 ohms-cmil/ft @ 68 F
Melting Point Liquid US1650 F
Melting Point Solid US1630 F
Modulas of Elasticity in Tension15000 ksi
Modulas of Rigidity5600 ksi
Specific Gravity8.41
Specific Heat Capacity0.09 Btu/lb/°F @ 68 F
Thermal Conductivity67.0 BTU in/hr.ft2.°F @ 68 F

Sizes Available

HOLLOW RODSMin Bore Size 20 mm and Max OD 100 mm
ROUND RODS/RODS6mm To 130 mm
HEX5mm To 60mm
SQUARE4mm To 60mm
FLAT5mm Min Thickness and max Width 120mm
PROFILES / SECTIONSAS per Customer Drawing
BILLETSUp to 200 mm
INGOTSAS per Specification